We expect lumber to perform as specified, but outside the lumber industry, few people understand how important it is to measure and manage its moisture content. Sawmills need to measure lumber moisture carefully and continuously at key stages of the manufacturing process to get the best lumber quality. Poor moisture management can cost a sawmill hundreds of thousands of dollars a year. Our calcolatore per eccessiva e insufficiente essiccazione can help you estimate what it’s costing your mill.
Incoming: Sorting “Green” Lumber in the Sawmill
Although it isn’t done as often as it should be, sorting lumber by moisture (and sometimes by total density) before it goes into the kiln can help optimize kiln schedules. Green sorting systems measure the moisture and/or density of green lumber so each piece can be assigned to a drying category (fast, medium, or slow).
Green sorting has three main advantages. First, it lets you categorize lumber accurately for essiccazione in forno, so kiln operators can predict drying times more accurately. Second, it can shorten overall drying times, because fast-drying lumber can be dried together instead of being mixed with slow-drying packs. Third, it reduces drying degrade from overdrying and underdrying. When a mill starts green sorting, the financial benefits can begin right away.
Il processo di essiccazione: misurazione dell'umidità in forno
Quality control (QC) is especially important during kiln drying. For years, technology has let kiln operators place moisture measurement probes inside the lumber packages in the kiln. These probes send real-time moisture data to kiln control software on a computer, so operators can monitor moisture content in the kiln as the lumber dries.
With that data, operators can develop moisture-based drying schedules for better quality and more efficient drying, and better determine when to stop the kiln. In-kiln moisture measurement systems can also reduce the need for manual “hot checks.” Managing moisture content at this stage adds to the mill’s profitability by making the process more efficient.
Planer Mill: misurazione in linea dell'umidità del legname essiccato
Sistemi di misurazione dell'umidità in linea in the planer mill are the most important tools for capturing moisture data on every piece of lumber. They give QC personnel, especially those working on kiln drying, the data they need to improve the drying process. Without them, mills are very limited in how accurately they can analyze their drying.
Drying lumber well is part science and part art, and in-line moisture data is the science that helps kiln operators perfect the art.
Download gratuito: come scegliere un sistema di misurazione dell'umidità per la tua segheria - Guida all'acquisto
Acquista il sistema Omega In-Line
In qualità di Responsabile Vendite di Wagner Meters, Ron vanta oltre 35 anni di esperienza nella strumentazione e nei sistemi di misura in diversi settori. In precedenti incarichi, ha ricoperto il ruolo di Responsabile Vendite Regionale, Responsabile Prodotti e Progetti e Responsabile Vendite per aziende produttrici di strumentazione di misura.
Ultimo aggiornamento il 12 ottobre 2026
Ciao Ron, stiamo cercando un misuratore di umidità per misurare l'umidità nei tronchi prima della cippatura. Tu e la tua azienda avete idee o prodotti che possano aiutarci? Grazie per il tuo aiuto, Ross.
Ross,
Wagner non dispone attualmente di alcuna strumentazione per questa applicazione. Perché è necessario farlo? Solo per curiosità.
Cordiali saluti,
Ron Smith, Wagner Meters
541.582.0541